Aluminium Extrusion Machining: Six Metres, One Table
Handemo Insight

Aluminium Extrusion Machining: Six Metres, One Table

Every few weeks a photograph arrives in our inbox: a six-metre aluminium extrusion lying across two trestles in a workshop, and a question underneath it that sounds simple. Can you machine this? The answer is yes. The machine is almost never what decides whether the job works. What decides it is that the part is three times longer than the table it has to sit on, and every decision after that — where you cut it, where you clamp it, which face goes first — follows from that one fact.

We build lathes and machining centres, so there is an obvious commercial answer to this question and it is not the one we usually give. On a large share of extrusion work the machine that earns the money is a saw, and the machining centre only drills holes. Splitting the job correctly between those two saves more than any choice between two models of machining centre ever will.

Double-column profile machining center frame with a long clamped bed, built for extruded aluminium profiles
Long beds exist for exactly this job. But a long bed is not the same thing as a straight part, and it is not the first decision to make.

This is one of our machining solution notes, written from what shops send us rather than from a catalogue. It covers extruded aluminium as a machining job: what the profile is like when it leaves the die, why six metres changes the arithmetic, how to hold a hollow section without closing it, why the flat you cut follows the bow that was already there, and where a saw should do the work instead of a spindle. If you machine steel weldments or castings, most of the clamping advice still reads across; the section stiffness part does not.

An Extrusion Is Not A Milled Part That Happens To Be Long

Aluminium extrusion arrives with a history. It was pushed through a die at around 500 °C, quenched, cut, and then stretched on a stretcher to straighten it — the trade calls it tension levelling. The stretching is what gives the profile its usable straightness, and it is also why the profile is never as relaxed as a rolled bar. Some of that stretch stays in the metal as a locked-in stress, and when you cut a window into a flange or remove one wall of a hollow section, the balance changes and the profile moves. On a short bracket nobody notices. On four metres of rail, everybody notices.

The second thing the die leaves behind is variation. A die wears. Wall thickness drifts along the length, the corners carry slightly different radii, and the profile has a bow that you can see if you put a straight edge along it on a flat floor. A T-slot rail with a 40 by 40 mm section is sold as a standard item, but two bundles from two suppliers are not the same part, and two bundles from the same supplier a year apart are not either.

Then there is the surface. Most architectural and automation profiles are anodised, which is a hard oxide skin grown out of the aluminium itself, a few hundredths of a millimetre thick. It is not paint. You cannot machine it and keep it, you cannot weld through it without stripping it, and a cut edge exposes bare metal that will oxidise differently from the faces around it. On a visible product that difference is what the customer sees first.

Put those three together — locked-in stress, die variation, a skin that cannot be cut — and the shape of the job changes. You are not removing metal to a drawing. You are deciding which features are made by the die, which by the saw, and which by the spindle, and then keeping the last group as small as it can be.

Six Metres On An Eight Hundred Millimetre Table

Here is the arithmetic that decides the machine, and it is worth doing before any model is discussed. Take a light rail, 6,000 mm long, with a row of holes on 150 mm pitch — 40 holes. Compare what happens on the travels we actually publish.

A VMC855 has 800 mm of X travel. A VMC1690 has 1,600 mm. A VMC1890 has 1,800 mm. With a sensible overlap so the tool does not start on a half-cut hole, the number of times the part has to be released, moved and located again works out at roughly seven on the 855 and three on the 1,890. Each of those moves is not one minute of machine time. It is a clamp and unclamp, a re-location against a stop or a previously cut feature, a check that the profile has not sprung, and — this is the part people forget — a fresh chance for the accumulated position of the holes to drift along the rail.

Diagram comparing how many times a six metre aluminium extrusion must be repositioned on 800, 1600 and 1800 mm X travel machines
Same part, same 40 holes. The only thing that changes between the three bars is how many times the profile leaves the table.

There are three honest ways to run this job, and they are not ranked by machine price.

The first is to saw the rail into handling lengths before it ever reaches a machine, and design the joint so that the cut is hidden inside a connector or a bracket. This is what most automation frame builders do, and it is why a 40 by 40 T-slot frame can be built in a garage with a chop saw and a drill press. It is also the right answer for anything that will be anodised afterwards, because the cut end can go through the anodising bath with everything else.

Long T-slotted bed of a profile machining center with an operator setting stops before a run
The long T-slotted bed of a profile machine. The stops on this bed are the fixture; the profile is only ever as good as the index they give it.

The second is step-and-repeat on a normal machine: clamp the whole rail on a fixture plate that overhangs the table, machine a window of features, release, slide, re-clamp, machine the next window. This works, it is how a lot of shops actually do it, and it fails in one specific way — every re-clamp is a new datum, and the datum is usually a previously machined hole rather than the extrusion itself. That is fine until one hole is drilled slightly off, because the next window inherits it.

The third is a machine with enough travel to hold the rail and reach all of it, which is what a double-column profile machine or a long-bed vertical centre is for. The VMC1890 at 1,800 mm of X reduces the job to three setups. A gantry machine can go further. The cost is floor space, foundation and money, and it only pays if the rail is a repeat product rather than a one-off.

Job shapeWhat actually decides itMachine that fits
T-slot frame, 2020 to 8080, cut and tapped onlySquareness of the cut end, not the spindleCold saw plus a drill or tapping spindle; a machining centre is optional
Rails up to about 1,500 mm with cross holes and pocketsWhether the whole rail fits inside the travelVMC855 or VMC1160 on a fixture plate
Rails 2 to 3 m with features along the full lengthNumber of repositions you are willing to pay forVMC1690 or VMC1890, long fixture, one or two moves
Rails over 3 m, or profiles with a deep sectionBed length and how the part is supported, not spindle powerDouble-column profile machine or gantry
Heat sink and housing profiles, short and deepTool reach into the fins, and chip evacuationHigh-speed vertical centre with a small taper

Clamping A Hollow Section Without Closing It

A 40 by 40 profile has walls around 1.5 to 2 mm. A machine vice will flatten it. That is not an exaggeration and it is not a question of being gentle with the handle — the section is a hollow box, and a box resists bending far better than it resists being squeezed across its opening. Clamp on the two open flanges and the flanges come together; release, and they spring back to somewhere near where they were, which is not necessarily where they were when you drilled.

So the clamping rule for extrusion is: clamp across a closed cell, never across an opening. On a T-slot profile the closed cell is the corner where two walls meet; on a hollow rectangular tube it is the diagonal. If there is no closed cell where you need to hold, the answer is a machined pocket in a soft jaw that touches the profile on two adjacent faces and a machined stop that touches the third, with the clamp pressure applied along the wall rather than through it.

Cross section diagram showing clamp force closing a hollow extrusion when applied across the opening, and holding it when applied across a closed corner
Same profile, same clamp. On the left the force is carried by the opening; on the right it is carried by the corner. Only one of them leaves the section where it started.

Support is the other half. A rail clamped at two points will sag between them, and the sag is not uniform because the profile's own bow pushes it one way or the other. Support every few hundred millimetres on adjustable stands, and set the stands to the part rather than setting the part to the stands. This is the single most common reason a long rail comes off the machine with holes that are in the right place along the rail but at the wrong height in the middle.

Pressure matters too, and it is easier to control than people expect. Most vices and fixtures will hold a profile at a fraction of the force needed for a steel block, provided the clamp is on a closed corner and the tool is sharp. If you find yourself increasing clamp pressure to stop chatter on an extrusion, the problem is usually that the tool is rubbing rather than cutting, or that the profile is unsupported underneath.

The Flat You Cut Follows The Bow That Was Already There

This is the part of extrusion work that catches experienced machinists, because it contradicts the instinct that a machined face is a true face.

A six-metre profile that looks straight against a wall will show a bow of a few millimetres when you lay a straight edge along it. The bow is not a defect; it is what tension levelling achieves at that length. Now clamp that profile flat onto a machine table. To make it sit flat you have to pull the bow out, which means the profile is now held under load — it is a spring, pinned at both ends. Machine a flat on it and release the clamps, and the flat is no longer flat: it has the bow back in it, because the metal returned to the shape it wanted.

There are only two ways out. Either you stress-relieve the situation by machining the profile in the condition it will live in — supported, not forced flat — or you accept that the machined face is a local feature and design the part so that the local feature is all that has to be true. That second option is what most good extrusion products do: the machined pocket locates an insert, and the insert's own face is what the assembly references. The rail's overall straightness is handled by the frame, not by the cut.

The same logic applies to cutting a slot down the length of a hollow profile. Take a wall out of one side and the section becomes asymmetric, and an asymmetric section bows as the stress rebalances. If the slot is long, expect the profile to curve towards the side that still has material, and plan the operation so the slot is cut before the features that reference it, not after.

Where The Saw Should Do The Work

For the largest single category of extrusion work — frame rail, cut to length, tapped at the ends, cross-drilled for connectors — the cut end is the most important surface on the part, and a saw makes it better than a milling cutter does.

A carbide cold saw cutting a 40 mm section leaves an end that is square enough to butt against another rail with a connector plate and close the joint by eye. It also cuts in seconds and needs no fixture. A milling cutter facing the same end has to hold a part that is six metres long and hanging off the table, and it will do the job more slowly and no better. Choosing a machining centre to face extrusion ends is a common way to spend money on the wrong operation.

The reverse mistake is just as common: sawing a part that needs a machined face. If the profile carries a bearing bore, a seal groove, a dovetail or a face that another component sits on, a saw cut is not a substitute, and no amount of deburring will make it one. The useful question is not "which is better" but "which faces on this drawing are doing locating work". Those get machined. Everything else gets sawed, and the saw is not a compromise.

One detail worth knowing: the two saw types behave differently at the cut. A cold saw with a carbide blade produces a cut face that is close to a machined face and needs only a deburr. A band saw produces a face with a visible blade mark and a slight burr on the exit side, which is fine for a joint that is covered by a connector and not fine for a visible end. If the design has visible cut ends, the saw choice is a design decision that happens before the machine choice.

The Anodising Order Is Not Negotiable

Anodising is the last operation, always, and it is the operation that most often forces a redesign when it is discovered late.

The oxide layer grows out of the surface, so anything machined after anodising has bare aluminium around it. On a black anodised rail, a drilled hole shows a bright ring. On a clear anodised rail, the cut edge oxidises to a slightly different tone over months. Neither is a fault in the machining; both are the consequence of an order of operations that cannot be reversed.

Two practical rules follow. First, decide before quoting whether the part is anodised, because it changes the deburring — a sharp edge under an anodised skin is a place the coating thins and fails, so edges that will be coated get a small break rather than a razor edge. Second, if the part must be anodised and then have a feature added, that feature should be a pressed insert, a tapped hole with a masked thread, or a connection made with a T-nut, not a cut. Masking is possible and it is charged for, so it belongs in the price rather than in the surprise.

Which Machine, For Which Extrusion Job

Reading the table above back in terms of the models we build: the small T-slot frame business does not need a machining centre at all, and if it also makes short brackets and plates, a VMC855 with 800 mm of travel covers both. Rails that fit inside 1,600 mm go on a VMC1690 and the job is one setup with a long fixture; the reasoning behind that machine's table and load rating is set out in the VMC1690 guide. Rails between 1,600 and 2,000 mm, which is a very common length for conveyor and machine-guard work, go on a VMC1890 and the arithmetic in the VMC1890 guide is the same arithmetic used above.

VMC1890 vertical machining center with 1800 mm X travel on the assembly floor at the Handemo plant
A long-bed vertical centre is the answer to the reposition count, not to the bow. The bow is handled by support and by the sequence.

Beyond 3 m the geometry stops being a vertical machine question. A double-column machine keeps the spindle close to the work over the whole length, which is what a long profile needs, and the trade-off against a gantry is floor space and how much of the length is really used. That comparison is in gantry versus vertical machining center. If the profiles are short but the features are deep — heat sinks, motor housings, LED bodies — the limiting factor is tool reach into fins and chip evacuation, and a small-taper high-speed spindle is worth more than a long table; the taper argument is in BT40 versus BT50.

For the thin-wall mechanics that dominate everything above, machining thin-wall parts covers the deflection side in more depth, and the busbar note covers a flat soft-metal job where the order of bending and machining decides the result — the same class of problem as the anodising order here. A worked example of a thin plate held without distortion is in the thin-wall motor plate case.

What To Send Us With An Extrusion Enquiry

We can answer the machine question in one pass, and the answer is often "you do not need what you asked for", if the enquiry carries five things.

  • The profile drawing with wall thickness, and the supplier's section tolerance if you have it — die variation is the number that decides how much material you can plan to remove.
  • The finished length, and whether the part is one piece at that length or several cut from one bar.
  • Which faces are doing locating work, marked on the drawing. That list, not the feature count, decides whether the job is a saw job, a drill job or a milling job.
  • Whether the part is anodised or painted, and whether the finish goes on before or after the features.
  • The condition the part is assembled in — supported along its length, or free-standing at the ends — because that decides whether the bow matters.

With those five we will tell you the smallest machine that does the job, or that a saw and a drill will do it and the money is better spent elsewhere. We would rather lose the machine sale than quote a long-bed centre for a frame business that needs a cold saw.

Handemo CNC machine assembly hall in Tengzhou, Shandong, with vertical machining centers in rows
Machines are built and run in before shipping in Tengzhou. If you send a profile sample with the drawing, the setup is proved on the actual section rather than on a drawing of it.

Questions We Get On Extrusion Work

Can you machine a six-metre extrusion at all?

Yes, but rarely in one clamping on a vertical machine. The usual routes are sawing to handling length and joining, step-and-repeat along a long fixture with the profile supported, or a double-column machine that holds the full length. Which one is right depends on how many parts the drawing has along the length and whether the profile is a repeat product.

Why did my holes line up on the bench and not in the assembly?

Because on the bench each rail was checked on its own, and in the assembly the rails reference each other. If the hole rows were machined in two or three repositions and the datum was a previously drilled hole rather than a fixed stop on the fixture, the error along the rail is cumulative. Check two rails against each other on a flat surface before blaming the machine.

Is it better to buy the profile cut to length from the supplier?

For frame rail, usually yes, if the supplier's saw is good and the cut ends are not visible. You lose the ability to machine a feature that references the cut end, and you pay freight on finish-length parts rather than on bars, so the calculation is about volume. For anything with a machined face near the end, keep the bar and control the cut yourself.

How do I stop a hollow profile closing in the vice?

Clamp across a closed corner or a closed cell, not across the opening, and use soft jaws machined to the section so the force is spread over two adjacent faces. Support the profile underneath at short intervals, and stop increasing clamp pressure to cure chatter — on a 2 mm wall, more pressure makes the chatter worse because the wall moves instead of the tool.

Does the extrusion need stress relieving before machining?

Not usually for frame work, because the features are small and local. It matters when you remove a significant part of the section along the length, such as a long slot in a hollow profile: the balance changes and the part will curve. In that case the fix is sequence — cut the slot first, then machine everything that references it — rather than heat treatment, which on a thin extruded section introduces its own distortion.

Can one machine do the sawing and the machining?

Some long-bed machines can carry a saw arbor, and for a dedicated product line that is a real saving because the part never leaves the fixture. For mixed work it is usually slower than a cold saw and it ties up the spindle. Most shops we work with keep the saw separate and use the machine for the features that genuinely need a spindle.

Start With The Drawing, Not The Machine

Send the profile drawing, the finished length and the list of faces that locate something, and we will come back with the operation split — what the die makes, what the saw makes, what the spindle makes — before we talk about a model. If the answer is a saw and a drill press, that is what we will say. If it is a VMC1890 with a long fixture, the arithmetic above is already the argument for it.

Upload your drawing or contact Handemo CNC directly. Email: sales1@handemocnc.com | WhatsApp: +86 135 6320 3038

Related reading in this series: all machining solutions, VMC1890 specifications, and VMC855 specifications.

CNC Machine Tools

Explore Our CNC Machines